dc.description.abstractRepassivation studies of four commonly used metals and alloys; iron, nickel, mild steel and stainless steel were carried out in 0.05M, 0.15M and 0.50M NaHC03 media at a pH of 8.3. The removal of the oxide film, under potentiostatic conditions was effected by means of a sapphire point mounted on a moving trolley attached to a perspex electrolytic cell. The resulting current time-transient was recorded on an oscilloscope and a strip chart recorder, and analysed to evaluate the kinetics of the repassivation process. The rate of removal of the passive film was 80+10 cm s-1. ...en_US
dc.identifier.urihttp://archive.cmb.ac.lk/handle/70130/6827
dc.language.isoenen_US
dc.publisherFaculty of Science, University of Colomboen_US
dc.titleRepassivation Studies of Some Mechanically Damaged Metal Surfacesen_US
dc.typeThesisen_US

Files

Original bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Ph.D 07.pdf
Size:
780.1 KB
Format:
Adobe Portable Document Format

License bundle

Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description:

Collections